Invar 36 Plate, Alloy 36 (Invar) / UNS K93603 / ASTM F1684 Hot Rolling , Forging

Product Details:
Place of Origin: China
Brand Name: JINXING
Certification: ISO 9001
Model Number: Invar 36 Plate
Payment & Shipping Terms:
Minimum Order Quantity: 10KGS
Price: 15~50USD/kg
Packaging Details: Plywood Case
Delivery Time: 25days
Payment Terms: L/C, D/A, D/P, T/T, Western Union
Supply Ability: 10000kgs/M

Detail Information

Material: UNS K93603 Standard: ASTM F1684
Surface: Pickled , Polished Characteristic: Low Expansion Alloys
Heat Treatment: Solution Annealed Density: 8.05g/cm3
High Light:

ni based superalloys

,

nickel based superalloys

Product Description

INVAR 36 Plate , Sheet

AMS l-23011 CL7MIL l-23011 CL7UNS K93602/03

4J36 (China), Fe-Ni36 (France), 1.3912, Ni36 (Germany), X1NiCrMoCu, N 25-20-7 (UK) Invar 36, UNSK93600 thermostat alloy, UNSK93601 pressure vessel sheet (USA)

 

Alloy 36 (Invar) / K93603 / ASTM F1684 Widely known under several trades names such as Invar* and Nilo 36**, this grade is a 36% nickel-iron alloy. It exhibits a near zero rate of thermal expansion from around 100oC up to 200oC. This is around a tenth of the expansion rate of carbon steels. Alloy 36 also demonstrates a high retention of strength and toughness at cryogenic temperatures, making it suitable for a variety of low temperature or low expansion applications.

The alloy is ideally suited to areas where dimensional changes due to temperature must be minimal, such as tooling for aerospace composites, radio and electronic devices and structural members in precision equipment such as lasers, measuring devices, thermostats and cryogenic instrumentation. Alloy 36 can also be utilised in combination with a high expansion material to crate mechanical movement with temperature in thermomechanical controls and switchgear.

 

Russia USA England Japan Franch Germany
36H Invar 36 Cactus LE Invar Standard Vacodil36 Nilo36

 

Content Composition %

C Si P S Mn Ni Fe
Less than%
0.05 0.30 0.020 0.020 0.20-0.60 35.0-37.0 Rest

 

Average linear expansion coefficient

Sample heat treatment system /(10-6/℃)
20-100℃ 20-300℃
The semi-finished sample is heated to 840C10C, kept for 1 h, water quenched, and then the sample is processed into a finished sample, which is kept at 315C10C for 1 h with furnace cooling or air cooling. ≤1.5 ---

 

Type Size/mm Deliver State
Bar 5.0-8.0 Cold Drawn
8.0-30.0 Hot rolling
30.0-180.0 Hot forging
Plate 3.5-30.0 Hot rolling
30.0-40.0 Hot forging
Strip 0.2-3.5 Cold rolling
Flat wire 0.5-5.0 Hot rolling
Round wire 0.1-5.0 Cold Drawn
Capillary OD8.0-1.0ID0.1-8.0 Cold Drawn
Pipe OD120-8.0, ID8.0-129 Cold drawn

Invar 36 is used in environments that require very low expansion coefficients.

 