WNiFe Tungsten Heavy Alloy Aviation Rod
Product Details:
|
|
Place of Origin: | CHINA |
---|---|
Brand Name: | JINXING |
Certification: | ISO 9001 |
Model Number: | 90WNiCu -Heavy Tungsten Alloy Drills |
Payment & Shipping Terms:
|
|
Minimum Order Quantity: | 10 kg |
Price: | Negotiable |
Packaging Details: | plywood cases |
Delivery Time: | 15-20 days |
Payment Terms: | L/C, T/T, D/P, Western Union |
Supply Ability: | 2000 kg per month |
Detail Information |
|||
Product Name: | Heavy Tungsten Alloy Drills | Grade: | 90WNiCu |
---|---|---|---|
Density: | 16.3-18.5 G/cc | Purity: | 90%W |
Tensile Strength: | 730-1400 MPa | Elongation: | <11% |
Standards: | ASTM B777-2010 | Applications: | Industrial Parts |
High Light: | Heavy Tungsten Alloy Drills,730 MPa Tungsten Alloy Drills,High Strength Tungsten Alloy Drills |
Product Description
Heavy Tungsten Alloy Drills are made of tungsten base (tungsten content is generally 80%~98%) and a small amount of nickel, iron, copper, cobalt, molybdenum, chromium and other elements. The density of high specific gravity tungsten alloy can reach 15.20 ~ 18.70g/cm3, also known as high specific gravity tungsten alloy or high density alloy material. Because tungsten alloy weighs more than twice as much as steel.
Tungsten alloy has a series of excellent properties, high specific gravity: General specific gravity 16.5-18.75g/cm3, high strength: tensile strength 700-1000mpa, strong light absorption: 30-40% higher than general lead specific gravity, high thermal conductivity: mold is 5 times that of steel; Low thermal expansion coefficient: the capacity is only 1 / 2 / 3 / 3 of that of steel, with good conductivity and resistance to welding and cutting.
The usual method for manufacturing heavy tungsten alloys is to mix the required tungsten, iron, nickel or copper powder, and then cold press the liquid phase to nearly full density. During the liquid phase treatment, the base tungsten alloy melts and part of tungsten enters the solution to form large tungsten particles (20 ~ 60 μ m) Microstructure of.
Chemical Composition | 90%W | 93%W | 95%W | 97%W | ||||||
State | Sinter | Vacuum | Forge | Sinter | Vacuum | Forge | Sinter | Vacuum | Sinter | Vacuum |
Density (g/cc) |
16.85-17.25 | 17.15-17.85 | 17.75-18.35 | 18.25- 18.85 | ||||||
Hardness (HRC) |
32 Max | 30 Max | 40 Min | 33 Max | 31 Max | 40 Min | 34 Max | 32 Max | 35 Max | 33 Max |
Tensile Strength (Max) | 770 Min | 900 Min | 1400 Max |
770 Min | 910 Min | 1440 Max | 735 Min | 920 Min | 700 Min | 850 Min |
Yield Strength (Mpa) |
620 Min | 620 Min | 1280 Max | 650 Min | 650 Min | 1340 Max | 650 Min | 650 Min | - | - |
Elongation (%) |
5 Min | 15 Min | 5 Min | 5 Min | 12 Min | 3 Min | 3 Min | 12 Min | 2 Min | 6 Min |