Burnishing Tungsten Nickel Iron Rod Wnife Heavy Tungsten Alloy

Product Details:
Place of Origin: China
Brand Name: JX
Certification: ISO
Model Number: Tungsten Nickel Iron Rod Bar Wnife Tungsten Heavy Metal Alloy Price Per Kg
Payment & Shipping Terms:
Minimum Order Quantity: 10kgs
Price: Negotiable
Packaging Details: standard packing
Delivery Time: 25days
Payment Terms: T/T
Supply Ability: 300kgs month

Detail Information

Size: As Request Quality: ISO9001:2008
Surface: Polishing,burnishing,black Surface Delivery Time: 25days
Packing: Standard Exporting Name: Tungsten Nickel Iron Rod Wnife Tungsten Heavy Metal Alloy Price Per Kg
High Light:

Burnishing Tungsten Nickel Iron Rod

,

Wnife Heavy Tungsten Alloy

Product Description

Tungsten Nickel Iron Rod Wnife Tungsten Heavy Metal Alloy Price Per Kg

Name:Tungsten Nickel Iron Rod

Material:W90-97NiFe(Magnetic)&W90-97NiCu(Nonmagnetic)
Density:16.8-18.8g/cm3

Property of tungsten alloy
AMST 21014 class 1
90%WNiFe, 90%WNiCu
Density : 17.0
Hardness: 32HRC max
Elongation: 5-20%


Tungsten Nickel Copper Alloy
Tungsten Nickel Iron Rod Method
1), Blending of tungsten powder with other metal powders and a bonding agent, cooling and sieving.
2), Pressing the blended powder to the required shape (allowing for shrinkage during the final processing), and shaping the green part component.
3). Pre-sintering the pressed components to remove the bonding agent.
Final sintering in the hydrogen fed furnace to fuse the powder particles together.
4). Supplied in bar, square, round and rectangle sizes are available in rough oversize, or turned or ground to exact requirements. Components can also be produced to customer drawings.

 

Tungsten Nickel Iron Rod Picture:

Burnishing Tungsten Nickel Iron Rod Wnife Heavy Tungsten Alloy 0Burnishing Tungsten Nickel Iron Rod Wnife Heavy Tungsten Alloy 1

 

Technical datasheet for Tungsten Nickel Iron Rod

Tungsten heavy alloy W-Ni-Fe W-Ni-Cu
Designation 90W 92.5W 95W 97W 90Cu 92.5Cu 97Cu
Density (g/cm3) 17.0 17.6 18.0 18.5 17.0 18.0 18.5
Tensile Strength (MPa) 820 780 820 840 750 650 550
Elongation (%) 10 7.0 7.0 5.0 1.2 1.0 0.5
Hardness (HRC) 25 26 27 28 24 27 28
Young's Modulus (GPa) 310 320 340 365 270 300 320
Thermal expansion coefficients (10-6/K) 4.61 4.62 4.60 4.50 5.60 4.40 4.00
Electrical conductivity (%) 10 13 13 17 17 19 23
Thermal conductivity (W/m.K) 80 90 93 95 110 120 125
 